Skip to main content

Table 3 Textural properties of ZrO2–CA, CeO2–CA, and CeZrO2–CA

From: Ce–Zr-based mixed oxide catalyst for oxidative depolymerization of kenaf stalk (biomass) into vanillin

Catalyst

Surface area

(m2/g)

Pore volume

(cm3/g)

Pore size

(nm)

ZrO2–CA

26

0.016

2.557

CeO2–CA

28

0.06

4.94

CeZrO2–CA

50

0.05

10.52