Table 2 The compositional analysis of untreated MDF and the solid contents after ICSE pretreated

From: Impact of moisture content on instant catapult steam explosion pretreatment of sweet potato vine

 

Cellulose/%

Hemicellulose/%

Lignin and ash/%

Untreated

 MDF

16.83 (1.86)

9.60 (1.20)

42.88 (0.67)

Pretreated

 FF

40.25 (1.62)

10.27 (0.13)

22.39 (0.52)

 NDF

41.10 (2.18)

10.92 (0.90)

19.66 (2.91)

 MDF

41.96 (4.66)

8.23 (1.40)

24.76 (1.86)

 SF-2

42.28 (1.75)

10.95 (1.96)

23.88 (4.41)

 SF-30

48.69 (1.35)

15.04 (0.92)

20.40 (1.85)

 SF-60

48.38 (0.31)

15.95 (0.86)

21.28 (2.77)

  1. Data were shown as “mean (standard deviation)”