Skip to main content

Table 2 Onset temperature (Tonset), degradation temperature on maximum weight-loss rate (Tmax), weight loss (WL) for CPF and the obtained CNC

From: Preparation and characterization of cellulose nanocrystal extracted from Calotropis procera biomass

Samples

Cellulose thermal degradation

Carbonic residue degradation

Tonset (°C)

Tmax (°C)

WL (%)

Tonset (°C)

Tmax (°C)

WL (%)

Calotropis procera fiber

277

330

79

420

510

31

Obtained CNC

180

205

57

367

406

43