Skip to main content
Fig. 6 | Bioresources and Bioprocessing

Fig. 6

From: Maximizing production of cellulose nanocrystals and nanofibers from pre-extracted loblolly pine kraft pulp: a response surface approach

Fig. 6

XRD diffraction patterns of original biomass (red line), bleached Kraft pulp (green line), CNCs (purple line) from high CNC yielding conditions (i.e., run 4–60% w/w acid, 60 min, 55 °C, 40 mesh) and CNFs (cyan line) from high CSR yielding conditions (i.e., run 17–54% w/w acid, 45 °C, 90 min, 20 mesh)

Back to article page