Skip to main content

Table 5 Thermal conductivity of CPCMs-4, CPCMs-4 with 1% EG, CPCMs-4 with 3% EG, and CPCMs-4 with 5% EG

From: Enhanced thermal conductivity of waste sawdust-based composite phase change materials with expanded graphite for thermal energy storage

Samples

Thermal conductivity (W/(m))

CPCMs-4

0.1156 ± 0.0016

CPCMs-4 + 1%

0.1202 ± 0.0022

CPCMs-4 + 3%

0.1371 ± 0.0029

CPCMs-4 + 5%

0.1431 ± 0.0011