Table 5 Glass transition temperature (Tg) of UFPNR

From: Ultrafine fully vulcanized natural rubber modified by graft-copolymerization with styrene and acrylonitrile monomers

Sample

Monomer contents (phr)

ST/AN ratio (wt%)

Irradiation dose (kGy)

Tg (°C)

Unmodified NR

–

–

–

− 64

Unmodified UFPNR

–

–

300

− 63

UFPNR-g-(PS-co-PAN)

5

50/50

300

− 62

UFPNR-g-(PS-co-PAN)

15

50/50

300

− 62